A methylvinyl silicone rubber and a room-temperature vulcanized(RTV) graft silicone rubber were studied with the positron annihilation technique. It is shown that τ 1 and τ 2 for the RTV rubber are longer than those in the former
but τ 3 is shorter than these for the former. A qualitative explanation for the facts is given.