在通过核反应
24
Mg(
d
α
)
22
Na制备
22
Na时,我们曾考虑用MgO作靶,因此研究了电泳法制备MgO薄层的条件。选用丙酮作介质,用超声波发生器制备了MgO的比较稳定的悬浮体,以Pt片作阳极,以Cu片为阴极进行电泳,研究了电泳的电压、产额(
Y
)和悬浮液浓度(
C
)、电泳时间(
t
)的关系以及一些添加剂对薄层的影响。
The conditions for preparation of MgO layers with electrophoresis are introduced. Taking acetone as medium
and Pt and Cu plates as electrodes
we found the optimum voltage(150 volts) and concentration of the suspension (10mg/ml). The maximum yield and the thickness of the layers obtained are 60 mg and 15 mg/cm
2
respectively. The quality of the layers is rather satisfactory.
Danish Patent , 67277 ( 1943 ).
U. S. Patent , 2442863 ( 1944 ).
S. Bjrnholm et al . , Nucl. Instr. Meth ., 5 , 196 ( 1959 ).
V. Verdingh and K. F. Lawer , Nucl. Instr. Meth ., 60 , 125 ( 1968 ).
G. P. Gutierrez et al . , J. Electrochem. Soc ., 109 ( 1962 ).
0
浏览量
31
下载量
0
CSCD
关联资源
相关文章
相关作者
相关机构
京公网安备11010802024621