Simulation method for secondary hydriding breakage of zirconium alloy cladding
NUCLEAR ENERGY SCIENCE AND ENGINEERING | 更新时间:2024-10-25
    • Simulation method for secondary hydriding breakage of zirconium alloy cladding

    • “In the field of nuclear reactors, experts have designed a zirconium alloy cladding tube secondary hydrogen embrittlement simulation device, which successfully simulates the oxidation and hydride generation processes on the inner and outer walls of the cladding tube, providing a solution to the problem of secondary hydrogen embrittlement.”
    • NUCLEAR TECHNIQUES   Vol. 45, Issue 4, Article number: 040602(2022)
    • DOI:10.11889/j.0253-3219.2022.hjs.45.040602    

      CLC: TL99
    • Received:10 December 2021,

      Revised:14 March 2022,

      Published:15 April 2022

    移动端阅览

  • MA Yan,ZHANG Zhixin,CHEN Jiawei.Simulation method for secondary hydriding breakage of zirconium alloy cladding[J].NUCLEAR TECHNIQUES,2022,45(04):040602-040602. DOI: 10.11889/j.0253-3219.2022.hjs.45.040602.

  •  
  •  

0

Views

43

下载量

1

CSCD

Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Study on corrosion behavior of metallic uranium surface treated with CO
Microstructure of GaAs/AlAs/GaAs with and without oxidation
Analyses of the IBAD MoS2-Ta films by TEM and energyspectrum techniques
Investigation of surface modification of the ion-implanted GH903 alloy

Related Author

Jiawei CHEN
Zhixin ZHANG
Yan MA
邹觉生
YANG Jiangrong ZOU Juesheng WANG Haifeng WANG Xiaohong WANG Jiayong
王海峰
王晓红
王嘉勇

Related Institution

中国工程物理研究院
China Academy of Engineering Physics
Institute of Physics & Condensed Physics Center, the Chinese Academy of Sciences, Beijing 100080) ZHENG Wenli JIA Quanjie JIANG Xiaoming
中国科学院高能物理研究所
0